Linerboard made of virgin pulp is called kraftliner, however recycled linerboard is known as testliner. Testliner is used for the outer and intermediate plies of corrugated board. Its printability is very good. Testliner is produced from 100% recyclable and made from renewable resources, with coloring agents providing a stable optical colour. It is available in different colour shades like golden yellow, natural shade and brownes shade. BF range of test liner from 22 to 35. GSM ranges from 140 to 300.
GSM | BF | Bursting Strength | RCT (KN/m) | Moisture | Cobb 60 Sec | |
---|---|---|---|---|---|---|
gm/m2 | Kpa | Kg/cm2 | MD | CD | (%) | gm/m2 |
120 | 22 | 2.75 | 0.90 | 0.75 | 7 ± 0.5 | 35 to 40 |
140 | 22 | 3.08 | 1.20 | 1.00 | 7 ± 0.5 | 35 to 40 |
150 | 22 | 3.30 | 1.30 | 1.05 | 7 ± 0.5 | 35 to 40 |
180 | 22 | 3.96 | 1.90 | 1.50 | 7 ± 0.5 | 35 to 40 |
200 | 22 | 4.40 | 2.00 | 1.60 | 7 ± 0.5 | 35 to 40 |
220 | 22 | 4.84 | 2.10 | 1.80 | 7 ± 0.5 | 35 to 40 |
250 | 22 | 5.50 | 3.00 | 2.50 | 7 ± 0.5 | 35 to 40 |
300 | 22 | 6.60 | 3.10 | 2.80 | 7 ± 0.5 | 35 to 40 |
GSM | BF | Bursting Strength | RCT (KN/m) | Moisture | Cobb 60 Sec | |
---|---|---|---|---|---|---|
gm/m2 | Kpa | Kg/cm2 | MD | CD | (%) | gm/m2 |
120 | 24 | 2.88 | 1.00 | 0.80 | 7 ± 0.5 | 35 to 40 |
140 | 24 | 3.36 | 1.30 | 1.10 | 7 ± 0.5 | 35 to 40 |
150 | 24 | 3.60 | 1.40 | 1.20 | 7 ± 0.5 | 35 to 40 |
180 | 24 | 4.32 | 1.90 | 1.60 | 7 ± 0.5 | 35 to 40 |
200 | 24 | 4.80 | 2.60 | 2.00 | 7 ± 0.5 | 35 to 40 |
220 | 24 | 5.28 | 2.80 | 2.20 | 7 ± 0.5 | 35 to 40 |
250 | 24 | 6.00 | 3.40 | 2.80 | 7 ± 0.5 | 35 to 40 |
300 | 24 | 7.20 | 3.60 | 3.00 | 7 ± 0.5 | 35 to 40 |
GSM | BF | Bursting Strength | RCT (KN/m) | Moisture | Cobb 60 Sec | |
---|---|---|---|---|---|---|
gm/m2 | Kpa | Kg/cm2 | MD | CD | (%) | gm/m2 |
120 | 28 | 3.36 | 1.10 | 0.90 | 7 ± 0.5 | 35 to 40 |
140 | 28 | 3.92 | 1.40 | 1.20 | 7 ± 0.5 | 35 to 40 |
150 | 28 | 4.20 | 1.50 | 1.30 | 7 ± 0.5 | 35 to 40 |
180 | 28 | 5.04 | 2.00 | 1.70 | 7 ± 0.5 | 35 to 40 |
200 | 28 | 5.60 | 2.80 | 2.20 | 7 ± 0.5 | 35 to 40 |
220 | 28 | 6.16 | 3.00 | 2.40 | 7 ± 0.5 | 35 to 40 |
250 | 28 | 7.00 | 3.80 | 3.20 | 7 ± 0.5 | 35 to 40 |
300 | 28 | 8.40 | 4.00 | 3.40 | 7 ± 0.5 | 35 to 40 |
GSM | BF | Bursting Strength | RCT (KN/m) | Moisture | Cobb 60 Sec | |
---|---|---|---|---|---|---|
gm/m2 | Kpa | Kg/cm2 | MD | CD | (%) | gm/m2 |
120 | 35 | 4.20 | 1.30 | 1.10 | 7 ± 0.5 | 35 to 40 |
150 | 35 | 5.25 | 1.90 | 1.50 | 7 ± 0.5 | 35 to 40 |
180 | 35 | 6.30 | 2.60 | 2.00 | 7 ± 0.5 | 35 to 40 |
200 | 35 | 7.00 | 3.40 | 2.60 | 7 ± 0.5 | 35 to 40 |
220 | 35 | 7.70 | 3.60 | 2.80 | 7 ± 0.5 | 35 to 40 |
As Per Tappi Standard Tappi T 410
As Per Tappi Standard Tappi T 403
As Per Tappi Standard Tappi T 403
As Per Tappi Standard Tappi T 441
As Per Tappi Standard Tappi T 822
As Per Tappi Standard Tappi T 412
Finish Deckle 4250mm
Burst Factor 22 - 35 BF
GSM 120 - 300 GSM